por | Jul 17, 2026
Dental glass ceramics, Main ingredients are Lithium Disilicate, through special process. HT–High Transparency. HT– A1, A2, A3,B1,B2, BL1, BL2, BL3, BL4,C1,C2. Bending strength The average biaxial bending strength after being fully crystallized is 637Mpa,...
por | Jul 17, 2026
HT Blocks: Ideal forveneers, anterior crowns, and thin-wall restorations where maximum aesthetics are critical. The sale of this item may be subject to regulation by the U.S. Food and Drug Administration and state and local regulatory agencies.
por | Jul 17, 2026
Chemical Solubility: 30.3 μg/cm⁻². Why Choose This Block?. Composition: SiO₂ (61-71%), Li₂O (11-17%), ZrO₂ (1-5%), other oxides (6-30%). Radioactivity: <0.019 Bq/g (significantly below safety thresholds).
por | Jul 17, 2026
Size: C14 (18x13x15mm). Bending strength The average biaxial bending strength after being fully crystallized is 637Mpa, higher than the standard strength value, set by ISO6892:2008 For Dental Ceramics.